Measures to improve film adhesion strength
Film stress is an essential factor affecting the adhesion strength of the film layer. Film stress is divided into thermal and internal stress, and internal stress is divided into deposition internal stress and additional internal stress.
Since metal vapor molecules are combined with the substrate at high temperatures, thermal stress will inevitably be generated if the thermal expansion coefficients of the evaporation material and the substrate are different. Deposition internal stress is generated during the film formation process due to the large amount of heat released by gas phase atoms during the condensation process and the accumulation and contraction of grains when deposited on the substrate. Additional internal stress is generated when the film is exposed to the atmosphere after it is made or the atmosphere is introduced into the vacuum chamber, causing the film to oxidize.
The thermal stress, deposition internal stress, and additional internal stress of the film will generate a shear stress between the interface of the film layer and the substrate. When the shear stress is greater than the adhesion between the interface of the film layer and the substrate, the film layer will crack, warp, or fall off. Therefore, the reasonable matching of film materials and substrates can reduce the thermal stress of the film. The correct formulation of the film deposition process can minimize the internal stress or make the stresses compensate for each other. This is a crucial measure to improve the film adhesion strength.
In addition, it is necessary to avoid the influence of humid gas, oil pollution, and dust on the film adhesion strength. In the case of moisture or oil pollution, the surface of the substrate will adsorb a layer of water molecules or oil molecules. In this way, it is difficult for the evaporated metal vapor molecules to directly produce physical adsorption with the substrate and even more challenging to produce chemical adsorption. Instead, they can only adhere to the water molecule or oil molecule layer adsorbed by the substrate, weakening the adhesion strength between the film layer and the substrate interface. The dust attached to the substrate hinders the adsorption of the evaporated metal vapor molecules to the substrate. Sand holes (or pinholes) without the film layer are formed where the dust is—the more dust attached to the substrate, the more serious the sand holes.
The following measures are used to improve the film adhesion strength.
Increase substrate temperature
The baking temperature of the substrate or workpiece cannot be the same as the working temperature of the evaporation source. Otherwise, the vapor molecules of the evaporating material will evaporate again after reaching the substrate or workpiece, resulting in the undesirable effects of difficult film formation and coarse grains.
Choose the right working pressure
When coating aluminum films, it is recommended to maintain a vacuum chamber pressure of approximately 10-2 PaPa to ensure optimal film quality.
The substrate needs to be carefully treated before coating
During production, try to avoid stopping the machine midway and filling the air multiple times to prevent the airflow with impurities from rushing to the substrate surface, causing the film layer to lose adhesion.
Specific requirements for substrate
Choose the appropriate film thickness
Before film formation, the substrate is bombarded and heated with electrons or ions.
Contact Us
Discuss Your Custom Glass Project
Share your drawing, photos or dimensions, together with the intended use and target quantity. We will review your requirements and discuss the next steps.
Sales Enquiries
Email sales@bo-glass.com with your part description, intended use and target quantity.
Send Your Design
Use the form to upload a drawing or describe an existing part. Mark critical dimensions and tell us which surfaces or features matter most.
Request a Custom Glass Quote
Upload a drawing or share dimensions, quantity, intended use and finish. Include any heat, pressure or chemical exposure.
Your drawings remain confidential.
We use the contact details you provide to respond to your enquiry. See our Privacy Policy for more information.